Designation
Name |
The value |
Designation GOST Cyrillic |
06Х18Н11 |
Designation GOST Latin |
06X18H11 |
Transliteration |
06H18N11 |
By chemical elements |
06Cr18Н11 |
Name |
The value |
Designation GOST Cyrillic |
ЭИ684 |
Designation GOST Latin |
EI684 |
Transliteration |
EhI684 |
By chemical elements |
- |
Description
06KH18N11 steel is used: for the manufacture of welded equipment operating in environments of increased aggressiveness (the solutions of nitric, acetic acids, alkaline solutions and salts); for structures to be welded by spot welding.
Note
Steel corrosion resistant austenitic class. Steel 06KH18N11 has a lower content of ferrite phase than that of steel grade 08CR18NI10TI.
Standards
Name |
Code |
Standards |
Test methods. Packing. Marking |
В09 |
GOST 11878-66 |
Classification, nomenclature and General rules |
В30 |
GOST 5632-72 |
Blanks. Of the workpiece. Slabs |
В31 |
OST 3-1686-90 |
Bars and shapes |
В32 |
TU 14-11-245-88 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
V |
Ti |
Mo |
W |
GOST 5632-72 |
≤0.06 |
≤0.02 |
≤0.035 |
≤2 |
17-19 |
≤0.8 |
10-12 |
Rest |
≤0.3 |
≤0.2 |
≤0.2 |
≤0.3 |
≤0.2 |
Fe is the basis.