Steel 015Х16Н15М3

Designation

Name The value
Designation GOST Cyrillic 015Х16Н15М3
Designation GOST Latin 015X16H15M3
Transliteration 015H16N15M3
By chemical elements 015Cr16Н15Mo3

Description

015Х16Н15М3 steel is used: for manufacture of pipelines, working in conditions of boiling phosphoric, sulfuric, 10% acetic acid and sulfuric acid environments, designed for long service life at the operating temperature to 600 °C.

Note

Steel corrosion resistant austenitic class.

Standards

Name Code Standards
Steel pipes and fittings to them В62 TU 14-3-219-89

Chemical composition

Standard C S P Mn Cr Si Ni Fe N Ti Mo Co
TU 14-3-219-89 ≤0.015 ≤0.015 ≤0.02 ≤0.6 15-17 ≤0.015 14-16 Rest ≤0.015 ≤0.01 2.5-3 ≤0.02
Fe is the basis.

Technological properties

Name The value
Corrosion resistance 015Х16Н15М3 steel has higher resistance to pitting than steel 0ЗХ17Н14М3.