Alloy ХН67МБЮ (ЭП782)

Designation

Name The value
Designation GOST Cyrillic ХН67МБЮ
Designation GOST Latin XH67MBJu
Transliteration HN67MBYu
By chemical elements CrNi67CuBeAl
Name The value
Designation GOST Cyrillic ЭП782
Designation GOST Latin EP782
Transliteration EhP782
By chemical elements -

Description

Alloy ХН67МБЮ used: for the manufacture of various parts in turbine construction operating at temperatures up to + 700−750 °C.

Note

High-temperature Nickel-based alloy.
The recommended maximum operating temperature for a long time +750 °C, for a limited time +800 °C.
The temperature of beginning of intensive scaling in air +950 °C.

Standards

Name Code Standards
Blanks. Of the workpiece. Slabs В31 TU 14-1-1214-75
Bars and shapes В32 TU 14-1-2705-79