Alloy ХН54КВМТЮБ (JEP962P)

Designation

Name The value
Designation GOST Cyrillic ХН54КВМТЮБ
Designation GOST Latin XH54KBMTJuB
Transliteration HN54KVMTYuB
By chemical elements CrNi54CoВCuTeAlBe
Name The value
Designation GOST Cyrillic ЭП962П
Designation GOST Latin EP962P
Transliteration EhP962P
By chemical elements -

Description

Alloy ХН54КВМТЮБ used: for the manufacture of critical products.

Note

The granulated heat-resistant Nickel alloy.

Standards

Name Code Standards
Non-ferrous metals, including rare, and their alloys В51 GOST Р 52802-2007

Chemical composition

Standard C S P Mn Cr Si Ni Fe Al V B Ti Mo W Co Mg Hf La
GOST Р 52802-2007 0.04-0.08 ≤0.009 ≤0.015 ≤0.5 12-15 ≤0.5 Rest ≤0.5 3.6-4 0.1-0.6 0.015 2.4-3 3.9-5 2.4-3 8-10 0.02 0.1-0.4 0.01
Ni is the basis.
According to GOST R 52802-2007, the total content of niobium + tantalum should be within the range of 3.20-3.70%. Elements of boron, lanthanum and magnesium are introduced by calculation and chemical analysis is not determined. Deviations of the chemical composition according to the content are allowed: iron - plus 0.30%, aluminum - plus 0.20%, tungsten - plus 0.80%. Tantalum is not determined by chemical analysis. The content of residual elements in the finished alloy is in accordance with GOST 5632.