Description
40Х17СЛ steel is used: for the manufacture of hinged cast chains for rotary kilns, consisting of high-temperature or heat-resistant parts applied in the middle area when the temperature of the gas stream in the range of 500−900 °C.
Note
Heat-resistant steel.
Standards
Name |
Code |
Standards |
Castings with special properties (iron and steel) |
В83 |
TU 4112-07507311-010-02 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Fe |
TU 4112-07507311-010-02 |
0.3-0.5 |
≤0.03 |
≤0.045 |
0.5-1 |
16-18 |
1-2.5 |
Rest |
Fe is the basis.