Steel 07KH17N16TL

Designation

Name The value
Designation GOST Cyrillic 07Х17Н16ТЛ
Designation GOST Latin 07X17H16TL
Transliteration 07H17N16TL
By chemical elements 07Cr17Н16Ti

Description

07KH17N16TL steel is used: for the production of shaped casting parts for critical applications, and requirements for low magnetic susceptibility, high corrosion resistance and good machinability.

Note

Steel casting corrosion resistant austenitic class. Steel has a low magnetic susceptibility, high resistance against gas and intergranular corrosion, good machinability.

Standards

Name Code Standards
Steel castings В82 GOST 977-88

Chemical composition

Standard C S P Mn Cr Si Ni Fe Ti
GOST 977-88 0.04-0.1 ≤0.02 ≤0.035 1-2 16-18 0.2-0.6 15-17 Rest 0.005-0.15
Fe is the basis.

Mechanical properties

Section, mm sT|s0,2, MPa σU, MPa d5, % y, % KCU, kJ/m2
Quenching in water from 1050-1100 °C
100 ≥196 ≥441 ≥40 ≥55 ≥392

Description mechanical marks

Name Description
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σU Limit short-term strength
d5 Elongation after rupture
y The relative narrowing
KCU Toughness