A32 Steel

Designation

Name The value
Designation GOST Cyrillic A32
Designation GOST Latin A32
Transliteration A32
By chemical elements A32

Description

A32 steel is used: for the production of plate, universal broadband, bandpass and shaped rolled, intended for the manufacture of shells and other welded structures of ships and floating structures.

Note

High-strength steel.

Standards

Name Code Standards
Sheets and strips В23 GOST 5521-93, TU 14-1-4264-87

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu N As Al Mo
GOST 5521-93 ≤0.18 ≤0.035 ≤0.035 0.9-1.6 ≤0.2 0.15-0.5 ≤0.4 Rest ≤0.35 ≤0.008 ≤0.08 0.015-0.06 ≤0.08
Fe is the basis.
According to GOST 5521-93, the mass fraction of nitrogen is allowed up to 0.012%, provided that KCU ≥ 294 kJ / m 2 is provided in the rolled product after mechanical aging at 20 ° C. It is allowed in place of aluminum soluble in acids, to determine its total mass fraction, while the rate increases by 0.005%. Partial replacement of aluminum with titanium is allowed: the total mass fraction of aluminum and titanium should be at least 0.015%, the mass fraction of titanium - not more than 0.020%, the mass fraction of aluminum soluble in acids - not less than 0.005%. The microalloying of niobium and (or) vanadium steel to 0.05 and 0.10%, respectively, or other grain refining admixtures is permitted in agreement with the consumer.

Mechanical properties

Section, mm sT|s0,2, MPa σU, MPa d5, %
Castings according to GOST 2685-75
≥315 440-590 ≥22

Description mechanical marks

Name Description
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σU Limit short-term strength
d5 Elongation after rupture