Incoloy welding

Difficulties in welding

Incolloy welding has a number of difficulties due to the fact that during the transition of metal from solid to liquid state there is a tendency for the formation of pores. During argon arc welding, nitrogen is the main source of pores. After the weld cools, nitrogen gas forms pores inside the metal.

Crystallization cracks

Incolloy welding is associated with a high propensity for the weld to develop crystallization cracks at the boundaries of large grains, which have a transcrystalline structure. To prevent cracking, it is necessary to limit the content of harmful impurities and introduce elements that bind sulfur into the most refractory compounds.

Alloy Ni Cr Cu Mo Mn Al Ti Nb C Si P S Fe
Inconel X-750 73,0 18,0 --- --- --- ≤0,8 ≤2,5 ≤0,9 ≤0,04 --- --- --- 6,8
Incolloy 800
30-35 19-23 --- --- --- 0.15 - .6 --- --- ≤0,1 0.15 - .6 --- --- 39.5 min
Incolloy 825
38-46 20-23,5 ≤3 2,5-3,5 ≤1 0,2 0,6-1,2 --- ≤0,05 ≤0,5 ≤0,03 ≤0,03 basis

Optimization of welding

Important condition is the cleanliness of welding materials surface and base metal as well as the binding of hydrogen. This is solved by the introduction of strong deoxidants into the weld pool (titanium, aluminum, etc.), as well as by the use of coatings or fluxes that can convert hydrogen into stable volatile compounds.

Furnizor

Supplier Evek GmbH offers to buy welded incolloy at a price that is optimal in this segment of rolled products. We offer welded incolloy for industrial applications from specialised warehouses of Evek GmbH. Timely delivery is ensured by representatives in Eastern European cities.

Buy, bargain price

Supplier offers to buy welded industrial application incolloy, price - due to technological features of production without including additional costs. The website of the company Evek GmbH contains information about the latest arrivals of products. The price is optimal from the supplier.