Designation
Name |
The value |
Designation GOST Cyrillic |
Р6М5К5 |
Designation GOST Latin |
P6M5K5 |
Transliteration |
R6M5K5 |
By chemical elements |
- |
Description
R6M5K5 steel is used: for the manufacture of roughing to semi-finishing tool used in the processing of superior alloy and stainless steels.
Note
Steel has a high tendency to decarburization.
Standards
Name |
Code |
Standards |
Bars and shapes |
В22 |
GOST 1133-71, GOST 2590-2006, GOST 2591-2006 |
Sheets and strips |
В33 |
GOST 4405-75 |
Bars and shapes |
В32 |
GOST 7417-75, GOST 14955-77, GOST 19265-73, TU 14-11-245-88 |
Steel wire medium and high carbon |
В72 |
TU 14-1-2783-79 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
V |
Mo |
W |
Co |
GOST 19265-73 |
0.86-0.94 |
≤0.03 |
≤0.03 |
0.2-0.5 |
3.8-4.3 |
0.2-0.5 |
≤0.6 |
Rest |
≤0.25 |
1.7-2.1 |
4.8-5.3 |
5.7-6.7 |
4.7-5.2 |
Fe is the basis.
Mechanical properties
Section, mm |
sT|s0,2, MPa |
σU, MPa |
d5, % |
y, % |
Rolled steel. Delivery condition |
|
≥510 |
≥850 |
≥12 |
≥14 |
Description mechanical marks
Name |
Description |
sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σU |
Limit short-term strength |
d5 |
Elongation after rupture |
y |
The relative narrowing |
Physical characteristics
Temperature |
Е, HPa |
G, HPa |
r, kg/m3 |
l, W/(m · °C) |
R, Mr. · m |
0 |
220 |
83 |
8200 |
- |
458 |
20 |
220 |
- |
8200 |
- |
458 |
100 |
- |
- |
- |
27 |
- |
200 |
- |
- |
- |
28 |
- |
300 |
- |
- |
- |
29 |
- |
400 |
- |
- |
- |
30 |
- |
500 |
- |
- |
- |
32 |
- |
600 |
- |
- |
- |
36 |
- |
700 |
- |
- |
- |
34 |
- |
900 |
- |
- |
- |
29 |
- |
A description of the physical symbols
Name |
Description |
Е |
The normal elasticity modulus |
r |
Density |
l |
Coefficient of thermal conductivity |
R |
UD. the resistivity |
Technological properties
Name |
The value |
The temperature of forging |
Start - 1160 °C, the end - 850 °C. |
Sanding behaviour |
good |
Viscosity |
good |
Wear resistance |
increased |