Cast iron CHS13

Designation

Name The value
Designation GOST Cyrillic ЧС13
Designation GOST Latin ChC13
Transliteration ChS13
By chemical elements ZrС13

Description

Cast iron CHS13 used: for the manufacture of parts with high corrosion resistance in concentrated acids, alkaline solutions, salts (except hydrofluoric and fluoride) at temperatures up to 200 °C (the simple configuration details of centrifugal and reciprocating pumps, compressors and valves, pipes and fittings to valves, heat exchangers and other items of chemical equipment).

Note

Siliceous high-alloy corrosion-resistant cast iron in liquid medium. It is not allowed to sharply variable and shock loads and temperature changes.

Standards

Name Code Standards
Castings with special properties (iron and steel) В83 GOST 7769-82

Chemical composition

Standard C S P Mn Si Fe
GOST 7769-82 0.6-1.4 ≤0.07 ≤0.1 ≤0.8 12-14 Rest
Fe is the basis.

Mechanical properties

σU, MPa HB, MPa
Castings on OST 1 90077-72
≥100 290-390

Description mechanical marks

Name Description
σU Limit short-term strength
HB Brinell hardness number