Designation
Name |
The value |
Designation GOST Cyrillic |
10ГС2 |
Designation GOST Latin |
10GC2 |
Transliteration |
10GS2 |
By chemical elements |
10MnС2 |
Description
10GS2 steel is used: for the manufacture of reinforcement steel classes At600, At600c, At600k, At800, designed for conventional reinforcement and prestressed concrete structures
Note
Steel low alloy structural manganese.
Standards
Name |
Code |
Standards |
Bars and shapes |
В22 |
GOST 10884-94 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
As |
GOST 10884-94 |
0.08-0.14 |
≤0.045 |
≤0.045 |
1-1.5 |
≤0.3 |
1.6-2.1 |
≤0.3 |
Rest |
≤0.3 |
≤0.08 |
Fe is the basis.
Mechanical properties
Section, mm |
sT|s0,2, MPa |
σU, MPa |
d5, % |
Reinforcing steel in the delivery state after the electric heating up to 400 °C according to GOST 10884-94 (the Holy column of the delivery condition specified strength class) |
10-40 |
≥600 |
≥800 |
≥12 |
10-32 |
≥800 |
≥1000 |
≥8 |
Description mechanical marks
Name |
Description |
sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σU |
Limit short-term strength |
d5 |
Elongation after rupture |
Technological properties
Name |
The value |
Weldability |
Welded without any restrictions. |