Designation
Name |
The value |
Designation GOST Cyrillic |
50Х25Н35В5К15С |
Designation GOST Latin |
50X25H35B5K15C |
Transliteration |
50H25N35V5K15S |
By chemical elements |
50Cr25Н35W5Co15С |
Description
50Х25Н35В5К15С steel is used: for the manufacture of pipes tsentrobezhnolityh for the manufacture of the coils of the tubular furnace installations production of ammonia, hydrogen, ethylene, carbon disulphide, etc., operating in the temperature range 760−1060 °C and a pressure of 3.92 MPa (40 kgf/cm2).
Standards
Name |
Code |
Standards |
Steel pipes and fittings to them |
В62 |
TU 1333-047-00220302-02 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
As |
V |
Ti |
Mo |
Zn |
Sn |
Pb |
W |
Co |
TU 1333-047-00220302-02 |
0.45-0.55 |
≤0.02 |
≤0.025 |
0.0005-0.71 |
25-28 |
1.1995-1.59 |
34-37 |
Rest |
≤0.2 |
≤0.01 |
0.0005-0.2 |
0.0005-0.1 |
≤0.5 |
≤0.01 |
≤0.01 |
≤0.01 |
4.5-5.5 |
14-16 |
Fe is the basis.
Mechanical properties
sT|s0,2, MPa |
σU, MPa |
d |
y, % |
Tsentrobezhnolityh pipe outer diameter 85-320 mm. Quenching in water or air from 1100-1150 °C |
≥245 |
≥490 |
≥4 |
≥5 |
Description mechanical marks
Name |
Description |
sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σU |
Limit short-term strength |
d |
Elongation after rupture |
y |
The relative narrowing |