Designation

Name The value
Designation GOST Cyrillic 7Х2СМФ
Designation GOST Latin 7X2CMF
Transliteration 7H2SMF
By chemical elements 7Cr2СMoV

Description

7Х2СМФ steel is used: for the manufacture of forged work rolls for cold rolling of metals.

Chemical composition

Standard C S P Mn Cr Si Ni Fe V Mo
0.7-0.8 ≤0.03 ≤0.03 0.6-1 1.7-2.2 0.7-1 ≤0.5 Rest 0.15-0.3 0.35-0.6
Fe is the basis.

Technological properties

Name The value
The temperature of forging Start - 1200 °C, the end - of 800 °C.