Cast iron CHH2
Designation
Description
Cast iron CHH2 used: for the manufacture of parts with high corrosion resistance to the gas, air and alkaline media in terms of friction and wear and heat-resistant in air up to 600 °C (the grate beams and horn for sinter machines, the details of the contact devices of chemical equipment, the grid of tube furnaces of oil refineries, parts for turbochargers, parts steklomassy).
Note
Heat-resistant low-alloy chromium cast iron.
Standards
Chemical composition
Fe is the basis.
According to GOST 7769-82, nickel content is allowed up to 1.0% or copper up to 1.50%, introduced by natural alloyed iron, alloyed with steel scrap or magnesium-containing ligature.
According to GOST 7769-82, nickel content is allowed up to 1.0% or copper up to 1.50%, introduced by natural alloyed iron, alloyed with steel scrap or magnesium-containing ligature.